MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond FS482 Long Pot Life High Tg Fiber Optic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND FS-482 is a dark blue, low viscosity epoxy adhesive developed for fiber-optic bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other optical components. It is recommended for laminating, bonding, and sealing applications using biconic and other F/O connectors where excellent wetting, long pot life and improved impact strength properties are required. This two-part epoxy adhesive is easily mixed at room temperature, remains at less than 3,000 cps at 25°C (maximum) for 40 minutes (minimum) and develops strong, tough bonds to glass and glass fibers, ceramics, many metals, and most rigid plastics. TRA-BOND FS-482 offers good mechanical impact and thermal shock resistance, and is also resistant to weather, water, gases and vapors, petroleum products, salts, and mild acids and alkalis.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 2250 cP2250 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Izod Impact, Notched 1.17 J/cm2.20 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.00e+8 ohm-cm9.00e+8 ohm-cm
Dielectric Constant 4.84.8
Dielectric Strength 16.9 kV/mm430 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
Pot Life 45 min45 min
 
Descriptive Properties
Color Dark Blue
Mix Ratio, parts by weight100/30Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F125 Fast Gel Clear Epoxy Adhesive
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive
Morgan Advanced Ceramics Cordierite

PTRAC289 / 71217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.