MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a room temperature cure) make 2115 an excellent choice for bonding optical components where alignment accuracy is essential. This high strength system is also used for laminating glass and rigid plastics or bonding metals and ceramics. TRA-BOND 2115 offers superior resistance to mechanical shock and temperature cycling. It has been used in cycling applications down to 4K. It is also resistant to water, weather, ozone, most petroleum products, mild acids and alkalis and many other chemicals.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccMixed
Viscosity 250 cP
@Temperature 25.0 °C
250 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878
Adhesive Bond Strength 26.2 MPa3800 psiLap shear, alum to alum
Izod Impact, Notched 0.117 J/cm0.220 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.00e+8 ohm-cm9.00e+8 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Dielectric Strength 16.9 kV/mm430 kV/in
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 55.0 °C131 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.551.55
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 120 min120 min
 
Descriptive Properties
Color Clear
Mix Ratio, parts by weight100/30Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive
Morgan Advanced Ceramics Cordierite
GBC Grade 92 Alumina
GBC Grade 90 Alumina
GBC Grade 85 Alumina

PTRAC016 / 70944

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.