MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silberline "A" Series A-1590FG
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: A-1590FG is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at low loading levels. This grade is not recommended for use with chromatic pigments, as it will not produce clean coloristic effects.

Applications: General Industrial

Key Words: ASTM D962-86 Type IV, Class A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/cc
Bulk Factor 0.0810.081
Volatiles 35 %35 %
Particle Size 6.0 µm6.0 µm
Particle Mesh Size <= 325 Mesh<= 325 Mesh0.1% retained
 
Descriptive Properties
SolventsMineral Spirits/High Flash

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UBE UPISEL-N BE1210 Copper Clad Laminate
Silberline A-6211
NuSil R-1600 Silicone One Part Sealing & Adhesive

ESIBER085 / 5840

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.