System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Adell AI-10 Nylon 66, Impact Modified
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Impact Grade
Material Notes:
Data provided by Adell Plastics, Inc.
Key Words:
Polyamide 66; Nylon 6,6; Adell Plastics, Inc.; Adell Nylon 6/6; Polyamide 6/6
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.09
g/cc
0.0394
lb/in³
ASTM D792
Water Absorption
1.2 %
1.2 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage
0.0125
cm/cm
0.0125
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
70
70
ASTM D785
Hardness, Rockwell R
112
112
ASTM D785
Tensile Strength, Ultimate
60.7
MPa
8800
psi
ASTM D638
Elongation at Break
60 %
60 %
ASTM D638
Flexural Strength
86.0
MPa
12500
psi
ASTM D790
Flexural Modulus
1.90
GPa
276
ksi
ASTM D790
Compressive Yield Strength
76.0
MPa
11000
psi
ASTM D695
Izod Impact, Notched
1.70
J/cm
3.18
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Melting Point
255
°C
491
°F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi)
177
°C
351
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
70.0
°C
158
°F
ASTM D648
Flammability, UL94
HB
HB
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Adell AI-30 Nylon 66, Impact Modified
Adell AD-30 Nylon 66, Ultra High Impact
Adell AD-10 Nylon 66, Ultra High Impact
Domo Technyl® A 246M Nylon 66, Impact Grade, EH50
DuPont Mobility and Materials Zytel® 444AHS BK152 PA66-I
PDEL38 / 29599
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.