MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC LUMIFLONĀ® LF-810 Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON LF-810 is a high molecular weight, low OH number fluoropolymer resin. It is meant to be formulated without crosslinkers, yielding coatings with extremely high weatherability and corrosion resistance. Potential applications for coatings made with LF-810 include architectural, industrial maintenance, and bridge coatings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/cc
Solids Content 45 %45 %
Viscosity 1764 cP1764 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.300.30[mg KOH/g]-polymer
 
Mechanical PropertiesMetricEnglishComments
Impact  0.50
@Diameter 12.7 mm
0.50
@Diameter 0.500 in
[m], Extrusion 0.5 kg; ASTM D2794
 >= 1.0
@Diameter 12.7 mm
>= 1.0
@Diameter 0.500 in
[m], Intrusion 0.5 kg; ASTM D2794
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.0<= 2.0
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min168 hour23
 
Descriptive Properties
AppearanceClear Liquid
HardnessHBPencil, ASTM D3363
OH Number4[mg KOH/g]-polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Lumiflon LF-810 Solvent Soluble Fluoropolymer
AGC Lumiflon LF-710F Solvent Soluble Fluoropolymer

PAGCX136 / 191245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.