MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Lumiflon LF-810 Solvent Soluble Fluoropolymer
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-810 is designed for use with mineral spirits for use in repair coatings and aged surfaces.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Solids Content 60 %60 %
Viscosity Measure 1300 - 3700 cSt1300 - 3700 cSt
Molecular Weight 20000 g/mol20000 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value 2.02.0
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 25.0 °C77.0 °F
 
Descriptive Properties
AppearanceTransparent
OH Value mg KOH/g38
SolventMineral Spirits

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Lumiflon LF-710F Solvent Soluble Fluoropolymer
AGC LUMIFLON® LF-810 Fluoropolymer Resin

PAGC06 / 22965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.