MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrotherm M-68 Structural Insulation Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make it well suited for a variety of applications.

Applications

  • Distribution boxes
  • Dams
  • Baffles
  • Launders
  • Troughs
  • Holding furnace linings

Advantages

  • Non-wetting
  • Excellent thermal insulation
  • Does not require insulation
  • Does not require pre-heating
  • Crack resistant
  • Shock resistant
  • Durable
  • Minimal shrinkage

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.089 g/cc0.03934 lb/in³
Loss On Ignition 4.6 %4.6 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0103 GPa1.49 ksi
Compressive Strength 22.1 MPa3210 psiat ultimate load
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.10 µm/m-°C
@Temperature 20.0 °C
3.94 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity  0.280 W/m-K
@Temperature 200 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.280 W/m-K
@Temperature 300 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 572 °F
 0.300 W/m-K
@Temperature 400 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.320 W/m-K
@Temperature 450 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 842 °F
Maximum Service Temperature, Air 788 °C1450 °FContinuous use
 816 °C1500 °F
Shrinkage  0.12 %
@Temperature 732 °C,
Time 86400 sec
0.12 %
@Temperature 1350 °F,
Time 24.0 hour
Length
 0.18 %
@Temperature 732 °C,
Time 86400 sec
0.18 %
@Temperature 1350 °F,
Time 24.0 hour
Width
 1.29 %
@Temperature 732 °C,
Time 86400 sec
1.29 %
@Temperature 1350 °F,
Time 24.0 hour
Thickness
 
Descriptive Properties
Screw Grip (Pull) Penetration Depth109 kg22 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Pyrocast ZR Refractory Shapes
Pyrotek Pyrocast ZI Refractory Shapes
Pyrotek Pyrocast ZG Refractory Shapes

CPYRO136 / 1858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.