MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Moplen RP315M Polypropylene Copolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen RP315M is a slightly modified polypropylene random copolymer. It contains slip and anti-blocking additives. Moplen RP315M is typically used for manufacturing of un-oriented cast films. Customers report stationary, lamination, textile and packaging of foodstuffs as typical applications. Moplen RP315M exhibits very good processability, and the films produced with Moplen RP315M exhibits good clarity, gloss and heat weldability. Applications: Food Packaging Film, Stationery Film, Textile Packaging Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 20.0 MPa2900 psiASTM D882
Film Elongation at Break, MD 730 %730 %ASTM D882
Coefficient of Friction 0.200.20ASTM D1894
 0.200.20ASTM D1894
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
1% Secant Modulus, MD 780 MPa113000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze <= 1.5 %
@Thickness 0.0500 mm
<= 1.5 %
@Thickness 0.00197 in
ASTM D1003
Gloss 88 %
@Thickness 0.0500 mm
88 %
@Thickness 0.00197 in
45°; ASTM D2457
 
Descriptive Properties
Processing MethodCast film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Purell RP315M Polypropylene

PEQT9093 / 220724

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.