MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Purell RP315M Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Purell RP315M is a medium modified polypropylene random copolymer for use in injection molding and film applications. Purell RP315M contains slip and anti-blocking agents. Purell RP315M is typically used for films and injection molding in healthcare applications. Applications: Caps & Closures (Healthcare), Healthcare Applications, Medical Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 45.0 MPa6530 psiISO 2039-1
Tensile Strength, Yield 30.0 MPa4350 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 11 %11 %ISO 527-1,-2
Tensile Modulus 1.10 GPa160 ksiISO 527-1,-2
Charpy Impact, Notched  0.200 J/cm²
@Temperature 0.000 °C
0.952 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 140 °C284 °FA50; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)H358/30
Processing MethodCast Film, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen RP315M Polypropylene Copolymer

PEQT8642 / 220276

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.