MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Taro® 20 DP SAE 30
Categories: Fluid; Lubricant

Material Notes: Texaco Taro 20 DP delivers value through:
  • Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lubricating oil controls cylinder liner wear effectively and protects bearings from corrosion. High performance antiwear additives provide excellent protection against adhesive wear for cams, camshaft and bearings.
  • Reduced foaming and improved water tolerance — Texaco Taro 20 DP provides a high degree of water tolerance and antifoam protection.
  • Prevents deposits — Provides exceptionally clean crankcase interiors, keeps oil control rings clean and prevents deposit formation throughout the engine. Extends oil filter cleaning intervals. Has excellent insolubles control.
  • Oxidation stability — Texaco Taro 20 DP withstands high thermal stress of high output trunk piston engines and reduces undercrown deposits. Lubricating qualities of the oil remain at a very high level over long periods of use and engine parts are protected from the corrosive effects of oil oxidation products.
  • Rust protection — Effective inhibitor package prevents corrosion of engine parts when the engine is not in operation.
  • Balanced additive combination — Ensures high quality performance with excellent overall protection. Provides minimum maintenance and down time, long engine life, and economical operating costs.

Texaco Taro 20 DP is a high performance high alkaline diesel engine oil for medium speed trunk piston diesel engines burning low sulphur heavy fuels or marine diesel oi (MDO).

Texaco Taro 20 DP is blended from high quality base oils and additives that provide an extra margin of protection against ring sticking, piston deposits and wear under the most severe operating conditions.

Taro20 DP has very good viscosity control when used in severe high temperature service and its excellent alkalinity retention characteristics prevent corrosive wear over long periods of operation. The unique detergent and dispersant additive system provides outstanding piston cleanliness as well as good heavy fuel related contaminants handling characteristics. This results in significant reduction of both "hot" (piston lands and grooves, piston undercrown, purifier preheaters) and "cold" (crankcase, cambox, rocker area, fuel pumps, purifier bowl) deposits.

Texaco Taro 20 DP is recommended for all types of trunk piston diesel engines burning MDO or low sulphur heavy fuels with a sulphur content up to 2%.

Texaco Taro 20 DP meets the requirements of all major marine diesel engine manufacturers.

Texaco Taro 20 DP meets the performance requirements of API Service Category CF.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 233036; MSDS Number: 8753

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 28.4 °28.4 °
Viscosity Measurement 102102Viscosity Index
Kinematic Viscosity at 40°C (104°F) 94 cSt94 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt11 cSt
Ash 2.05 %2.05 %Sulfated Ash, mass %
 
Chemical PropertiesMetricEnglishComments
Total Base Number 2020ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -18.0 °C-0.400 °F
Flash Point 240 °C464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 1400 Antifoam
Dow 1410 ANTIFOAM
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil AD
ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded

WTEXA190 / 77069

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.