MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam agent.

Chevron Aero Engine Oils Uncompounded do not contain ashless dispersant additives that retard the formation of sludge.

Chevron Aero Engine Oils Uncompounded are designed for the lubrication of aircraft piston engines where a straight mineral oil is recommended.

Applications

Chevron Aero Engine Oils Uncompounded are the type of oil recommended by most engine manufacturers and engine rebuilders for use as a break-in oil for new,rebuilt or overhauled four-stroke cycle aircraft piston engines. Check with the engine manufacturer or overhaul facility for their specific recommendation. They fully meet the requirements of SAE J1966, which has replaced MIL-L-6082E as the standard for nondispersant oils.

Key Words: CPS Number: 247308; MSDS Number: 7023
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 28.9 °28.9 °
Viscosity Measurement 9393Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 233 cSt233 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 19.2 cSt19.2 cStASTM D445
Ash 0.00 %0.00 %Sulfated Ash wt%
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °FASTM D97
Flash Point 288 °C550 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 1400 Antifoam
Dow 1410 ANTIFOAM
ChevronTexaco AFP White Oil
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil AD

WCHEV094 / 74709

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.