MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® H62 Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® H62 is a single component, electrically insulating, and thermally conductive epoxy adhesive. It may be used for heat-sinking semiconductor, hybrids, or electronic circuits.

Advantages & Application Notes:

  • Black and opaque appearance; it can block out light in opto-electronic devices.
  • Semiconductor encapsulant for COB packaged die. It may be used as a glob top DAM around the chip.
  • SMD “staking” material or Surface Mount Adhesive (SMA). The SMA may be used for double-sided PCB bonding of components; staking caps and resistors to ceramic or hybrid circuits. High viscosity adhesive paste has enough wet “green strength” to hold SMD’s to the PCB prior to cure.
  • Alternatives are available in different viscosity ranges and colors.
  • Excellent adhesion to ferrous and non-ferrous metals, glass, ceramics, PCB, and most plastics.
  • Thixotropic paste appearance makes it capable of syringe dispensing techniques, stencil or screen printing, or hand applications by brush or spatula.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/cc
Particle Size <= 50 µm<= 50 µm
Viscosity 17000 - 27000 cP
@Temperature 23.0 °C
17000 - 27000 cP
@Temperature 73.4 °F
10 rpm
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 136 ppm136 ppm
Ionic Impurities - K (Potassium) 28 ppm28 ppm
Ionic Impurities - Cl (Chloride) 55 ppm55 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Modulus 4.5273 GPa656.63 ksiStorage
Shear Strength 4.14 MPa600 psiLap
 >= 35.2 MPa>= 5100 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 2.00e+13 ohm-cm>= 2.00e+13 ohm-cm
Dielectric Constant 4.65
@Frequency 1000 Hz
4.65
@Frequency 1000 Hz
Dissipation Factor 0.011
@Frequency 1000 Hz
0.011
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.0 µm/m-°C26.7 µin/in-°FBelow Tg
 119 µm/m-°C66.1 µin/in-°FAbove Tg
Thermal Conductivity 0.500 W/m-K3.47 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 275 °C527 °FContinuous
 375 °C707 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 110 °C>= 230 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 436 °C817 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Transmission, Visible <= 1.0 %
@Wavelength 300 - 2500 nm
<= 1.0 %
@Wavelength 300 - 2500 nm
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
minimum
 60.0 min
@Temperature 120 °C
1.00 hour
@Temperature 248 °F
minimum
Pot Life 21600 min21600 min
Shelf Life 12.0 Month12.0 Monthrefrigerated
 
Descriptive Properties
ColorBlack, Opaque
ConsistencySmooth thixotropic paste
Ionic Impurities NH496 ppm
Number of ComponentsSingle
Thixotropic Index1.89
Weight Loss0.31%200°C
 0.42%250°C
 0.62%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silres® H62 C Silicone Resin
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin
Overview of materials for Brass
Aluminum 6061-O
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy

PPOXYT065 / 141104

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.