MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Permalyn™ 5095 Synthetic Resin
Categories: Polymer

Material Notes: Product Description: Permalyn™ 5095 Synthetic Resin, a pale, thermoplastic resin, is the glycerol ester of rosin. It is produced by a special process that yields a low-odor, low-acid-number resin that is suggested for use as a modifier for film-formers, elastomers, and waxes in various adhesives and protective coatings where pale color and minimal odor are required.

Application/Uses:

  • Asphalt Modification
  • Assembly
  • Automotive
  • Bookbinding
  • Building and Construction
  • Contact Adhesives
  • Footwear and Leather
  • Hot Melt Adhesives
  • Laminating
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
Key Attributes:
  • Low odor
  • Medium softening point
  • Resistant to thermal degradation
  • Thermoplastic resin
  • Very good color stability
  • Wide solubility and compatibility range

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Viscosity  150 cP
@Temperature 160 °C
150 cP
@Temperature 320 °F
Melt
 560 cP
@Temperature 140 °C
560 cP
@Temperature 284 °F
Melt
 3300 cP
@Temperature 120 °C
3300 cP
@Temperature 248 °F
Melt
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 8.08.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 88.0 °C190 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 3.03.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Evonik DS 50 Synthetic Resin
Evonik CA Synthetic Resin
Evonik AP Synthetic Resin

PEATM5498 / 222692

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.