Synthetic Resin AP is a neutral, unsaponifiable ketone-aldehyde condensation resin. It is generally used in combination with other binders. On account of its wide compatibility and its efficiency, it is used to improve gloss, solids content and covering capacity in the most diverse paint systems. |