MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper-Nickel, Chromium Bearing, UNS C72200
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Good hot and cold workability. Fabricated by forming, bending, and welding.

Applications: condenser and heat exchanger tubing, salt water piping.

Available as flat products and tube.

Key Words: Cupronickel with Cr
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 315 MPa45700 psiO61 temper
 480 MPa69600 psiH04 temper
Tensile Strength, Yield  125 MPa
@Strain 0.2 %
18100 psi
@Strain 0.2 %
O61 temper
 455 MPa
@Strain 0.2 %
66000 psi
@Strain 0.2 %
H04 temper
Elongation at Break 6.0 %6.0 %H04 temper
 46 %46 %O61 temper
Modulus of Elasticity 135 GPa19600 ksi
Poissons Ratio 0.230.23Calculated
Shear Modulus 55.0 GPa7980 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000264 ohm-cm
@Temperature 20.0 °C
0.0000264 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.8 µm/m-°C
@Temperature 20.0 - 300 °C
8.78 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.396 J/g-°C0.0946 BTU/lb-°F
Thermal Conductivity 34.5 W/m-K
@Temperature 20.0 °C
239 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1122 - 1176 °C2052 - 2149 °F
Solidus 1122 °C2052 °F
Liquidus 1176 °C2149 °F
Annealing Point 732 - 816 °C1350 - 1500 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 730 - 815 °C1350 - 1500 °F
Hot-Working Temperature 900 - 1040 °C1650 - 1900 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 0.30 - 0.70 %0.30 - 0.70 %
Copper, Cu 82 %82 %
Iron, Fe 0.50 - 1.0 %0.50 - 1.0 %
Manganese, Mn 0.40 - 0.90 %0.40 - 0.90 %
Nickel, Ni 15 - 18 %15 - 18 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.030 %<= 0.030 %
Titanium, Ti <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M50 Tool Steel
Ampco Metal AMPCO® 26 Aluminum Bronze, Forging
Geon® Performance Solutions Synplast™ 701P-N Di (C7-C11 Alkyl) Phthalate
Materion BrushForm® 158 Copper-Nickel-Tin Mill Hardened Strip (UNS C72900), TM10
AISI Type H13 Hot Work Tool Steel

MC72200b1 / 11839

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.