MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type M50 Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: Excellent resistance to softening up to about 425°C (800°F). Good oxidation resistance and high compressive strength characteristic of high-speed tool steels.

Applications: bearings and other parts for missiles aircraft engines; applications requiring high wear resistance and strength up to 425°C (800°F).

Key Words: UNS T11350
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.97 g/cc0.288 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 60 - 6560 - 65
 30
@Temperature 649 °C
30
@Temperature 1200 °F
 49
@Temperature 538 °C
49
@Temperature 1000 °F
 55
@Temperature 427 °C
55
@Temperature 800 °F
 58.5
@Temperature 316 °C
58.5
@Temperature 600 °F
 60.5
@Temperature 204 °C
60.5
@Temperature 400 °F
 62
@Temperature 93.3 °C
62
@Temperature 200 °F
 64
@Temperature -17.8 °C
64
@Temperature 0.000 °F
Hardness, Vickers  310
@Temperature 649 °C
310
@Temperature 1200 °F
 500
@Temperature 538 °C
500
@Temperature 1000 °F
 600
@Temperature 427 °C
600
@Temperature 800 °F
 680
@Temperature 316 °C
680
@Temperature 600 °F
 710
@Temperature 204 °C
710
@Temperature 400 °F
 750
@Temperature 93.3 °C
750
@Temperature 200 °F
 800
@Temperature -17.8 °C
800
@Temperature 0.000 °F
Fracture Toughness 13.2 - 19.8 MPa-m½12.0 - 18.0 ksi-in½cracks originating in case; case depth 0.30 to 0.35 in.
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.410 J/g-°C0.0980 BTU/lb-°F
Maximum Service Temperature, Air 482 °C900 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.77 - 0.85 %0.77 - 0.85 %
Chromium, Cr 3.75 - 4.25 %3.75 - 4.25 %
Cobalt, Co <= 0.25 %<= 0.25 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe >= 87.4 %>= 87.4 %As Balance
Manganese, Mn <= 0.35 %<= 0.35 %
Molybdenum, Mo 4.0 - 4.5 %4.0 - 4.5 %
Nickel, Ni <= 0.15 %<= 0.15 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.015 %<= 0.015 %
Tungsten, W <= 0.25 %<= 0.25 %
Vanadium, V 0.90 - 1.1 %0.90 - 1.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
M50-NiL High Performance Carburizing Bearing and Gear Steel
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel
ATI Allvac® M-50 Specialty Steel, Heat Treatment: 1107°C (2025°F) Q+T
Latrobe CM-50™ ASTM M50 High Speed Steel
AISI Type M42 Molybdenum High Speed Tool Steel (UNS T11342)

MSTM50A / 14103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.