MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.

Design/Construction:
Liner 1: Polyethylene
Side 1: Uncured Silicone Rubber
Substrate: Style 1080 Fiberglass
Side 2: Uncured Silicone Rubber
Liner: 2 Polyethylene

Product Use: Electrically insulating electronic adhesive. Bonds without primer.

Appearance: Blue colored, high viscosity gum.

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns1.50 milLiner 1
 38.1 microns1.50 milLiner 2
 63.5 microns2.50 milSide 1; Arlon SQA-TMS-003
 63.5 microns2.50 milSide 2; Arlon SQA-TMS-003
 76.2 microns3.00 milSubstrate; Arlon SQA-TMS-003
 203 microns8.00 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Silicone Property; ASTM D2240
Tensile Strength 5.17 MPa750 psiSilicone Property; ASTM D412
Elongation at Break 400 %400 %Silicone Property; ASTM D412
Poissons Ratio 0.500.50Approximately, Silicone Property
Shear Strength 2.76 MPa400 psiLap; ASTM 1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 39.0 kV/mm990 kV/inASTM D149
Dissipation Factor  0.0045
@Frequency 1e+6 Hz
0.0045
@Frequency 1e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
 0.0045
@Frequency 1e+6 Hz
0.0045
@Frequency 1e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FASTM E 831
CTE, linear, Transverse to Flow 20.0 µm/m-°C11.1 µin/in-°FASTM E 831
Specific Heat Capacity 0.980 J/g-°C0.234 BTU/lb-°FSilicone Property; E1461-01
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FProduct Property; ASTM E 1530
 0.400 W/m-K2.78 BTU-in/hr-ft²-°FSilicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg <= -100 °C<= -148 °FSilicone Property; ASTM D3418
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Pressure 0.0689 - 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 10.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
From date of manufacture
 
Descriptive Properties
ColorBlue
Total Product Weight (g/m2)240Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 73A Polyurethane, MDI PPG
Rogers Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Rogers Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate

PARL241 / 125427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.