MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 381 microns15.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585silicone property; ASTM D2240
Tensile Strength, Ultimate 2.07 MPa300 psisilicone property; ASTM D412
Elongation at Break 28 %28 %silicone property; ASTM D412
Modulus of Elasticity 0.0328 GPa4.75 ksisilicone property; Arlon SQA-TMS-008
Poissons Ratio 0.500.50silicone property
Shear Modulus 0.448 GPa65.0 ksisilicone property; ASTM D1002
Shear Strength 1.28 MPa185 psisilicone property; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
Dielectric Strength 31.5 kV/mm800 kV/inASTM D149
Dissipation Factor 0.0028
@Frequency 1e+6 Hz
0.0028
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
silicone property; ASTM E 831
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°Fsilicone property; ASTM E 1461-1
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°Fsilicone property; ASTM E 1530
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg -116 °C-177 °Fsilicone property; ASTM E 1356
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 7.22 °C
6.00 Month
@Temperature 45.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant
Rogers Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Overview of materials for Silicone Rubber
Overview of materials for Nylon 12
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

PARL045 / 79697

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.