MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: R/bak® materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/bak cushioning materials results in uniform quality printing over long run conditions. R/bak materials are available in a variety of length and thickness configurations.

R/bak SF and R/bak SS materials have an integrated polyester support layer to ensure dimensional stability and serve as a mounting base. R/bak U material is designed without the polyester support layer, and is recommended for cylinder build-up and spot cushioning. R/bak U1A is recommended for cylinder build-up, spot cushioning and spot coating applications for higher print quality.

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³ASTM D3574-95 Test A
Water Absorption 2.0 %2.0 %AMS 3568
 10 %10 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1212ASTM D2240
Hardness, Shore O 1717ASTM D2240
Tensile Strength >= 0.517 MPa>= 75.0 psiASTM D3573 Test E
Elongation at Break >= 100 %>= 100 %ASTM D3573 Test E
Compressive Yield Strength 0.0689 MPa
@Strain 25 %
10.0 psi
@Strain 25 %
Tear Strength >= 0.900 kN/m>= 5.14 pliASTM D624, Die C
Compression Set  <= 1.3 %
@Temperature 23.0 °C
<= 1.3 %
@Temperature 73.4 °F
ASTM D1667
 <= 3.3 %
@Temperature 70.0 °C
<= 3.3 %
@Temperature 158 °F
ASTM D3574

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group MM925 Condensation Cure 2-Part Molding Rubber
Multibase Multi-Flex® A 2504LC TPE Thermoplastic Elastomer
Carbon-Core CarbonFoam PU 2 R PU
BIW ASTM Class 2D0 Silicone Foam
CHT Group QM 2225 25 Shore A, Condensation Cure Moldmaking Material

PROGA944 / 138384

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.