MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H black is characterized by the following key-properties:
  • high stiffness and strength even after conditioning and over a wide temperature range
  • excellent notched impact resistance also at low temperatures
  • low creep
  • high heat distortion temperatures
  • low moisture absorption
  • very good dimensional stability and little warpage
The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement. Grivory GVL-5H black is used in the following market Segments:
  • automotive
  • mechanical engineering
  • household and appliances
The glass-fibres are aligned in parallel and are just as long as the pellets (usually 10 mm).

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³Dry; ISO 1183
Water Absorption 4.0 %4.0 %Sim. to ISO 62
Moisture Absorption 1.30 %1.30 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 270 MPa39200 psiConditioned; ISO 2039-1
 290 MPa42100 psiDry; ISO 2039-1
Tensile Strength at Break 230 MPa33400 psiConditioned; ISO 527-1/-2
 260 MPa37700 psiDry; ISO 527-1/-2
Elongation at Break 2.2 %2.2 %Dry; ISO 527-1/-2
 2.2 %2.2 %Conditioned; ISO 527-1/-2
Tensile Modulus 17.0 GPa2470 ksiConditioned; ISO 527-1/-2
 18.0 GPa2610 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 33.0 kV/mm838 kV/inDry; IEC 60243-1
 33.0 kV/mm838 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °FLong Term; ISO 2578
 220 °C428 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 220 °C428 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Exterior
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesLong Fiber Reinforced
 Partially aromatic Polyamide
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® GVL-6H nat PA*-GF60
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, Impact Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
Corning Gorilla® Glass 4 Touch Screen Glass

PGRH346 / 157055

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.