MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Triax® 1315 GF ABS + Polyamide Blend (DAM)
Categories: Polymer; Thermoplastic; ABS Polymer; Nylon (Polyamide PA)

Material Notes: Triax 1315 is an ABS (Acrylonitrile Butadiene Styrene) polyamide alloy with glass reinforcement for injection molding. Features: Excellent processability, Good chemical resistance, Excellent abrasion resistance, UL 94HB certified.

Applications: Housings, shrouds, Lawn and garden equipment, Automotive interior functional components, Automotive shrouds and housings, Power tools

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D 792
Melt Density 0.995 g/cc
@Temperature 240 °C
0.0359 lb/in³
@Temperature 464 °F
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0035 cm/cm0.0035 in/in
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
3.5 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 101101ASTM D 785
Tensile Strength, Yield 75.2 MPa10900 psiASTM D 638
Flexural Modulus 3.76 GPa545 ksiASTM D 790
Secant Modulus, MD 0.0462 GPa6.70 ksiASTM D 882
Izod Impact, Notched  0.694 J/cm
@Temperature -40.0 °C
1.30 ft-lb/in
@Temperature -40.0 °F
ASTM 256
 1.12 J/cm
@Temperature 23.0 °C
2.10 ft-lb/in
@Temperature 73.4 °F
ASTM 256
Puncture Energy 3.50 J
@Temperature -30.0 °C
2.58 ft-lb
@Temperature -22.0 °F
Energy to Maximum Force, FM- Penetration Test
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C25.0 µin/in-°FASTM D 696
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 20.0 °C
66.7 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.94 J/g-°C0.464 BTU/lb-°FMelt
Thermal Conductivity 0.155 W/m-K1.08 BTU-in/hr-ft²-°FMelt
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °Funannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 97.2 °C207 °Funannealed; ASTM D 648
Vicat Softening Point 200 °C
@Load 1.02 kg
392 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Gloss 26 %26 %at 60°, specular; ASTM D 523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 38.0 - 66.0 °C100 - 151 °F
Drying Temperature 88.0 °C
@Time 7200 - 14400 sec
190 °F
@Time 2.00 - 4.00 hour
Do not exceed 93°C
 
Descriptive Properties
Effective thermal diffusivity0.801E-7 m²/sMelt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
BASF Petra® 130 30% Glass Filled PET

PB10340 / 26378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.