MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Triax® 1315 GF ABS + Polyamide Blend (DAM)
Categories: Polymer; Thermoplastic; ABS Polymer; Nylon (Polyamide PA)

Material Notes: Triax 1315 is an ABS (Acrylonitrile Butadiene Styrene) polyamide alloy with glass reinforcement for injection molding. Features: Excellent processability, Good chemical resistance, Excellent abrasion resistance, UL 94HB certified.

Applications: Housings, shrouds, Lawn and garden equipment, Automotive interior functional components, Automotive shrouds and housings, Power tools

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D 792
Melt Density 0.995 g/cc
@Temperature 240 °C
Linear Mold Shrinkage, Flow 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0035 cm/cm
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 101ASTM D 785
Tensile Strength, Yield 75.2 MPaASTM D 638
Flexural Modulus 3760 MPaASTM D 790
Secant Modulus, MD 6.70 ksiASTM D 882
Izod Impact, Notched 1.30 ft-lb/in
@Temperature -40.0 °C
ASTM 256
 2.10 ft-lb/in
@Temperature 23.0 °C
ASTM 256
Puncture Energy 3.50 J
@Temperature -30.0 °C
Energy to Maximum Force, FM- Penetration Test
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µin/in-°FASTM D 696
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.94 J/g-°CMelt
Thermal Conductivity 0.155 W/m-KMelt
Deflection Temperature at 0.46 MPa (66 psi) 168 °Cunannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 97.2 °Cunannealed; ASTM D 648
Vicat Softening Point 200 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Gloss 26 %at 60°, specular; ASTM D 523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 270 °C
Mold Temperature 38.0 - 66.0 °C
Drying Temperature 88.0 °C
@Time 7200 - 14400 sec
Do not exceed 93°C
 
Descriptive Properties
Effective thermal diffusivity0.801E-7 m²/sMelt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
BASF Elastollan® C 70 A HPM TPUR
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
BASF Petra® 130 30% Glass Filled PET

PB10340 / 26378

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.