MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optimized for low phosphate release, to limit the formation of deposits on electrical contacts. The material has a red-brownish natural color.

Key characteristics:

  • Flame retardant, based on red phosphorous
  • Excellent mechanical performance
  • UL 94 V0 at 1.5 mm
  • UL 94 RTI 110°C at 1.5 mm
  • High CTI (600 V)
  • Brownish natural color

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ASTM D792, ISO 1183
Water Absorption 0.60 %0.60 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 4.5 %4.5 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inEuronil
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inEuronil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 160 MPa23200 psiISO 527, ASTM D638
Elongation at Break 2.5 %2.5 %
Tensile Modulus 11.0 GPa1600 ksiISO 527, ASTM D638
Flexural Yield Strength 250 MPa36300 psiISO 178, ASTM D790
 150 MPa
@Temperature 90.0 °C
21800 psi
@Temperature 194 °F
ISO 178, ASTM D790
Flexural Modulus 10.0 GPa1450 ksiISO 178, ASTM D790
 5.00 GPa
@Temperature 90.0 °C
725 ksi
@Temperature 194 °F
ISO 178, ASTM D790
Izod Impact, Notched (ISO)  8.50 kJ/m²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
533 kV/in
@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index  550 V
@Thickness 3.20 mm
550 V
@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
 550 V
@Thickness 3.20 mm
550 V
@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 248 °C478 °FISO 75, ASTM D648
Vicat Softening Point 257 °C495 °F49 N; ISO 306, ASTM D1525
 260 °C500 °F9.8 N; ISO 306, ASTM D1525
Flammability, UL94  V-1
@Thickness 0.800 mm
V-1
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 29 %29 %ASTM D2863
Glow Wire Ignition Temperature  775 °C
@Thickness 0.800 mm
1430 °F
@Thickness 0.0315 in
IEC 695-2-13
 825 °C
@Thickness 3.20 mm
1520 °F
@Thickness 0.126 in
IEC 695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 694-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 694-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 285 °C527 - 545 °F
Zone 1 260 - 280 °C500 - 536 °Fhopper
Zone 2 260 - 280 °C500 - 536 °F
Zone 3 270 - 280 °C518 - 536 °F
Zone 4 275 - 285 °C527 - 545 °F
Melt Temperature 275 - 290 °C527 - 554 °FDo not melt above 290°C
Mold Temperature 90.0 - 110 °C194 - 230 °FPreferred
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 4 hour4 hour
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi
 
Descriptive Properties
Clamping Forcein tons, 0.7 times the projected surface area in cm2
Flammability RatingSEFMVSS No. 302, 355x100x1 mm
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Holding Pressure90 MPa
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® AS V0 PA66
Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned
Celanese Hostaform® C9021 M Acetal Copolymer with Molybdenum Disulphide
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced

PLBN42 / 50431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.