MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This flame retardant material, U.L. 94 V0 rated at 0.8 mm, shows high Glow-wire, CTI values and good mechanical properties .It can be supplied in various colors. This grade is suitable for molding insulating parts for electrical devices: switches, rotary switches, timers and contactors. This product is available in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 78.0 MPa11300 psiISO 527 Type 1A
Elongation at Break 3.0 %3.0 %ISO 527 Type 1A
Tensile Modulus 7.00 GPa1020 ksiISO 527 Type 1A
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® AS V0 PA66
Domo TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Domo TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned
Celanese Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Celanese Hostaform® C9021 M Acetal Copolymer with Molybdenum Disulphide

PRHOD705 / 137936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.