MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllium Copper Nickel 72C Casting Alloy, Solution Treated and Aged
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Alloy 72C is a modified version of beryllium cupro-nickel alloy 71C, its increased beryllium content providing improved castability. Its field of application is the plastic tooling industry. Alloy 72C generally is ceramic mold cast into tooling used for molding flame-retardant plastics containing bromine, bromine-boron, chlorinated paraffins and phosphates, and other halogens. Additionally, alloy 72C tooling is resistant to corrosion by the foaming agents used in structural plastics that generate ammonia at elevated temperatures, as well as to decompositional products of PVC that contain HCI. The good casability of 72C allows it to be cast into tooling of fine detail.

Solution treated (water quenched from 995°C) and aged 3 hours at 510°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.60 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2626
Tensile Strength, Ultimate 860 MPa125000 psi
Tensile Strength, Yield 550 MPa79800 psi
Elongation at Break 70 %70 %in 50 mm
Modulus of Elasticity 150 GPa21800 ksi
Poissons Ratio 0.330.33
Machinability 40 %40 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 57.0 GPa8270 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000401 ohm-cm
@Temperature 20.0 °C
0.00000401 ohm-cm
@Temperature 68.0 °F
43% IACS, as-cast tempers
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 300 °C
8.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.337 J/g-°C0.0805 BTU/lb-°F
Thermal Conductivity 30.0 W/m-K
@Temperature 20.0 °C
208 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1065 - 1155 °C1949 - 2111 °F
Solidus 1065 °C1949 °F
Liquidus 1155 °C2111 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 995 °C1820 °F
Aging Temperature 510 °C950 °F
Casting Temperature 1200 - 1300 °C2190 - 2370 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.1 - 1.2 %1.1 - 1.2 %
Copper, Cu 68.8 %68.8 %
Iron, Fe 0.70 - 1.0 %0.70 - 1.0 %
Lead, Pb <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.70 %<= 0.70 %
Nickel, Ni 29 - 33 %29 - 33 %
Silicon, Si <= 0.15 %<= 0.15 %
Titanium, Ti 0.10 - 0.20 %0.10 - 0.20 %
Zirconium, Zr 0.10 - 0.20 %0.10 - 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® ELKON® 2140C Copper Tungsten Nickel material
Coronze Copper, UNS C63800, H08 Temper sheet/strip
Coronze Copper, UNS C63800, H06 Temper sheet/strip
NDZ-S, UNS C99500, Copper Casting Alloy
Nondezincification Alloy, UNS C99400, Copper Casting Alloy

MCUDEC02 / 11994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.