MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

North American Eastern Cottonwood Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Populus deltoides; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.370 g/cc0.0134 lb/in³Oven Dry Weight/Unseasoned Volume
 0.785 g/cc0.0284 lb/in³Unseasoned*
Cell Length 1.00 mm0.0394 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1500 N337 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1700 N382 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1900 N427 lb (f)Side
Tensile Strength, Ultimate 2.83 MPa410 psiPerpendicular to Grain*
 4.00 MPa580 psiPerpendicular to Grain
Modulus of Rupture 0.0365 GPa5.30 ksiStatic Bending*
 0.0590 GPa8.56 ksiStatic Bending
Flexural Yield Strength 20.0 MPa2900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 6.96 GPa1010 ksiStatic Bending*
 9.45 GPa1370 ksiStatic Bending
Compressive Strength 1.65 MPa240 psiPerpendicular to Grain*
 3.30 MPa479 psiPerpendicular to Grain
 12.2 MPa1770 psiParallel to Grain*
 15.7 MPa2280 psiMax Crushing Strength Parallel to Grain*
 34.0 MPa4930 psiParallel to Grain
Poissons Ratio 0.0180.018µTL, 12% Moisture Content
 0.0430.043µRL, 12% Moisture Content
 0.2920.292µTR, 12% Moisture Content
 0.3440.344µLR, 12% Moisture Content
 0.420.42µLT, 12% Moisture Content
 0.8750.875µRT, 12% Moisture Content
Shear Strength 4.69 MPa680 psiParallel to Grain*
 6.40 MPa928 psiOrientation Unknown
Impact 2.32.3in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 72007200psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00338 J/cm³0.490 in-lb/in³Static Bending*
Work to Maximum Load 0.0503 J/cm³7.30 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.102 W/m-K0.710 BTU-in/hr-ft²-°FOven Dry
 0.122 W/m-K0.850 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.9 %3.9 %Radial; Green to Zero Moisture
 9.2 %9.2 %Tangential; Green to Zero Moisture
 14.1 %14.1 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North American Black Willow Wood
North American Engelmann Spruce Wood
North American Elm Wood
American Red Maple Wood
American Chestnut Wood

PTSA100 / 71248

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.