MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

North American Black Willow Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Salix nigra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.390 g/cc0.0141 lb/inĀ³Air Dry (12-15% Moisture Content)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2.96 MPa430 psiPerpendicular to Grain*
 109 MPa15800 psiAxial
Modulus of Rupture 0.0540 GPa7.83 ksiStatic Bending
Flexural Modulus 7.00 GPa1020 ksiStatic Bending
Compressive Strength 3.00 MPa435 psiPerpendicular to Grain
 28.0 MPa4060 psiParallel to Grain
Shear Strength 8.60 MPa1250 psiOrientation Unknown
Toughness 23.8 J17.6 ft-lbRadial
 26.1 J19.3 ft-lbTangential
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.6 %2.6 %Radial; Green to Zero Moisture
 8.1 %8.1 %Tangential; Green to Zero Moisture
 14.4 %14.4 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North American Eastern Cottonwood Wood
North American Elm Wood
North American Engelmann Spruce Wood
American Chestnut Wood
American Red Maple Wood

PTSA080 / 71246

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.