MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General Purpose

Application: E&E (Housing)

CAS: 103598-77-2, 9003-56-9 and 181028-79-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 250 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.9 MPa
@Thickness 3.20 mm
7970 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 50 %
@Thickness 3.20 mm
>= 50 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 86.3 MPa
@Thickness 3.20 mm
12500 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.35 GPa
@Thickness 3.20 mm
341 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched 4.90 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
9.18 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 V
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.20 mm
30 - 60 sec
@Thickness >=0.0472 in
 30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
 30 - 60 sec
@Thickness >=2.00 mm
30 - 60 sec
@Thickness >=0.0787 in
High Amp Arc Ignition, HAI  30 - 60 arcs
@Thickness 1.20 mm
30 - 60 arcs
@Thickness 0.0472 in
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 2.00 mm
>= 120 arcs
@Thickness 0.0787 in
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
@Thickness 6.40 mm
198 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  60.0 °C
@Thickness >=1.20 mm
140 °F
@Thickness >=0.0472 in
 80.0 °C
@Thickness >=1.50 mm
176 °F
@Thickness >=0.0591 in
 80.0 °C
@Thickness >=2.00 mm
176 °F
@Thickness >=0.0787 in
 80.0 °C
@Thickness >=2.50 mm
176 °F
@Thickness >=0.0984 in
 80.0 °C
@Thickness >=3.00 mm
176 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  60.0 °C
@Thickness >=1.20 mm
140 °F
@Thickness >=0.0472 in
 80.0 °C
@Thickness >=1.50 mm
176 °F
@Thickness >=0.0591 in
 80.0 °C
@Thickness >=2.00 mm
176 °F
@Thickness >=0.0787 in
 80.0 °C
@Thickness >=2.50 mm
176 °F
@Thickness >=0.0984 in
 80.0 °C
@Thickness >=3.00 mm
176 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  60.0 °C
@Thickness >=1.20 mm
140 °F
@Thickness >=0.0472 in
 85.0 °C
@Thickness >=1.50 mm
185 °F
@Thickness >=0.0591 in
 85.0 °C
@Thickness >=2.00 mm
185 °F
@Thickness >=0.0787 in
 85.0 °C
@Thickness >=2.50 mm
185 °F
@Thickness >=0.0984 in
 85.0 °C
@Thickness >=3.00 mm
185 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=1.20 mm
V-0
@Thickness >=0.0472 in
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=2.00 mm
V-0
@Thickness >=0.0787 in
 V-0
@Thickness >=2.50 mm
V-0
@Thickness >=0.0984 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 5VB
@Thickness >=2.50 mm
5VB
@Thickness >=0.0984 in
 5VB
@Thickness >=3.00 mm
5VB
@Thickness >=0.118 in
 5VA
@Thickness >=1.50 mm
5VA
@Thickness >=0.0591 in
 5VA
@Thickness >=2.00 mm
5VA
@Thickness >=0.0787 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 260 °C446 - 500 °FInjection Molding
Middle Barrel Temperature 230 - 260 °C446 - 500 °FInjection Molding
Front Barrel Temperature 230 - 260 °C446 - 500 °FInjection Molding
Nozzle Temperature 250 - 265 °C482 - 509 °FInjection Molding
Melt Temperature 230 - 260 °C446 - 500 °FInjection Molding
Mold Temperature 50.0 - 70.0 °C122 - 158 °FInjection Molding
Drying Temperature 60.0 - 80.0 °C140 - 176 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant

PLAY586 / 148596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.