Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.19 g/cc | 1.19 g/cc |
Maximum Moisture Content | 0.020 | 0.020 |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0060 in/in @Thickness 0.126 in |
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 250 °C | 15 g/10 min @Load 4.76 lb, Temperature 482 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell R | 113 | 113 |
Tensile Strength, Yield | 62.8 MPa @Thickness 3.20 mm | 9100 psi @Thickness 0.126 in |
Elongation at Break | >= 80 % @Thickness 3.20 mm | >= 80 % @Thickness 0.126 in |
Flexural Yield Strength | 93.2 MPa @Thickness 3.20 mm | 13500 psi @Thickness 0.126 in |
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm | 384 ksi @Thickness 0.126 in |
Izod Impact, Notched | >= 6.08 J/cm @Thickness 3.20 mm, Temperature 23.0 °C | >= 11.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Arc Resistance | 60 - 120 sec | 60 - 120 sec |
Comparative Tracking Index | 250 - 400 V | 250 - 400 V |
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.20 mm | 30 - 60 sec @Thickness >=0.0472 in |
| 30 - 60 sec @Thickness >=1.50 mm | 30 - 60 sec @Thickness >=0.0591 in |
| 30 - 60 sec @Thickness >=2.00 mm | 30 - 60 sec @Thickness >=0.0787 in |
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.20 mm | 30 - 60 arcs @Thickness 0.0472 in |
| >= 120 arcs @Thickness 1.50 mm | >= 120 arcs @Thickness 0.0591 in |
| >= 120 arcs @Thickness 2.00 mm | >= 120 arcs @Thickness 0.0787 in |
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
|
Thermal Properties | Metric | English | Comments |
---|
Deflection Temperature at 0.46 MPa (66 psi) | 103 °C @Thickness 6.40 mm | 217 °F @Thickness 0.252 in |
UL RTI, Electrical | 60.0 °C @Thickness >=1.20 mm | 140 °F @Thickness >=0.0472 in |
| 80.0 °C @Thickness >=1.50 mm | 176 °F @Thickness >=0.0591 in |
| 80.0 °C @Thickness >=2.00 mm | 176 °F @Thickness >=0.0787 in |
| 80.0 °C @Thickness >=2.50 mm | 176 °F @Thickness >=0.0984 in |
| 80.0 °C @Thickness >=3.00 mm | 176 °F @Thickness >=0.118 in |
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.20 mm | 140 °F @Thickness >=0.0472 in |
| 80.0 °C @Thickness >=1.50 mm | 176 °F @Thickness >=0.0591 in |
| 80.0 °C @Thickness >=2.00 mm | 176 °F @Thickness >=0.0787 in |
| 80.0 °C @Thickness >=2.50 mm | 176 °F @Thickness >=0.0984 in |
| 80.0 °C @Thickness >=3.00 mm | 176 °F @Thickness >=0.118 in |
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.20 mm | 140 °F @Thickness >=0.0472 in |
| 85.0 °C @Thickness >=1.50 mm | 185 °F @Thickness >=0.0591 in |
| 85.0 °C @Thickness >=2.00 mm | 185 °F @Thickness >=0.0787 in |
| 85.0 °C @Thickness >=2.50 mm | 185 °F @Thickness >=0.0984 in |
| 85.0 °C @Thickness >=3.00 mm | 185 °F @Thickness >=0.118 in |
Flammability, UL94 | V-0 @Thickness >=1.20 mm | V-0 @Thickness >=0.0472 in |
| V-0 @Thickness >=1.50 mm | V-0 @Thickness >=0.0591 in |
| V-0 @Thickness >=2.00 mm | V-0 @Thickness >=0.0787 in |
| V-0 @Thickness >=2.50 mm | V-0 @Thickness >=0.0984 in |
| V-0 @Thickness >=3.00 mm | V-0 @Thickness >=0.118 in |
| 5VB @Thickness >=2.50 mm | 5VB @Thickness >=0.0984 in |
| 5VB @Thickness >=3.00 mm | 5VB @Thickness >=0.118 in |
| 5VA @Thickness >=1.50 mm | 5VA @Thickness >=0.0591 in |
| 5VA @Thickness >=2.00 mm | 5VA @Thickness >=0.0787 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F |
Middle Barrel Temperature | 235 - 255 °C | 455 - 491 °F |
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F |
Nozzle Temperature | 250 - 265 °C | 482 - 509 °F |
Melt Temperature | 235 - 265 °C | 455 - 509 °F |
Mold Temperature | 50.0 - 80.0 °C | 122 - 176 °F |
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F |
Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour |
Back Pressure | 0.0200 - 0.0600 MPa | 2.90 - 8.70 psi |
Screw Speed | 40 - 70 rpm | 40 - 70 rpm |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.