MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond MasterSil 170 Gel Two component, addition curing silicone gel for sealing, potting and encapsulation
Categories: Polymer; Thermoset; Silicone

Material Notes: Key Features:
  • Super soft upon curing
  • Convenient handling
  • Great optical clarity
  • Superb electrical insulator
Master Bond MasterSil 170 Gel is a two component, low viscosity silicone material for specialty potting and encapsulation. It is an addition cured system and does not require exposure to air for complete cross-linking. It has a forgiving one to one mix ratio by weight and will not outgas while curing. The system is 100% solids and contains no solvents. Upon mixing the viscosity is quite low and it has excellent flowability. It generates very little heat upon mixing and has a relatively long open time. MasterSil 170 Gel cures in 24-48 hours at ambient temperatures, or in 1-2 hours at 150-170°F. The system cures to be very soft, pliable and compliant with a hardness best measured by the penetration test method; for this system it is 65 mm. Upon curing, this silicone gel is transparent and is capable of withstanding temperatures ranging from -67°F to +392°F. It is capable of withstanding the most rigorous and extreme thermal shock and cycling without cracking or exerting stress on to components or substrates. These properties allow MasterSil 170 Gel to be used with sensitive or delicate optical and electronic parts. These components might be wire bonds, optical fibers, various chips, LEDs and resistors. Optically, the index of refraction is low and it transmits light very well from about 220-2,500 nm. This silicone gel can also be used in other types of applications where a low stress highly pliable sealant is needed. The properties of this system allow for relatively simple repairability.

Product Advantages:

  • Addition cured; no by-products released during cure; does not require air for curing
  • Low exotherm; very long pot life
  • Can cure in thicknesses beyond 1 inch
  • Very low shrinkage upon cure
  • Excellent optical clarity and transmission properties
  • Superior electrical insulation properties; highly resistant to water

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Viscosity 1000 cP1000 cPmixed
 
Mechanical PropertiesMetricEnglishComments
Penetration 6565[mm]
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.7
@Frequency 60 Hz
2.7
@Frequency 60 Hz
Dielectric Strength 19.7 kV/mm
@Thickness 3.17 mm
500 kV/in
@Thickness 0.125 in
Dissipation Factor 0.00020
@Frequency 60 Hz
0.00020
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.421.42
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.6 - 76.7 °C
1.00 - 2.00 hour
@Temperature 150 - 170 °F
 1440 - 2880 min
@Temperature 23.9 °C
24.0 - 48.0 hour
@Temperature 75.0 °F
Working Life 120 - 240 min120 - 240 minAfter mixing, 100 g batch
Shelf Life 6.00 Month6.00 MonthIn original unopened containers
 
Descriptive Properties
Mixing Ratio1:1Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 157 Two component, addition curing silicone for potting, encapsulation and sealing
Master Bond MasterSil 151 Two Component Low Viscosity Silicone Compound
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Vitro Minerals WhiteLite™ 32 Lightweight Mineral Powder
Vitro Minerals WhiteLite™ 42 Lightweight Mineral Powder

PMASTM728 / 233785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.