MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vitro Minerals WhiteLite™ 42 Lightweight Mineral Powder
Categories: Ceramic; Oxide

Material Notes: WhiteLite™ Lightweight Mineral Powders are high brightness, synthetic aluminosilicate products for high performance filler and extender applications. With a specific gravity of 2.46, WhiteLite™ engineered powders are 10-17% lighter in weight than traditional naturally mined mineral fillers, which allows greater volumetric extension when used in coatings and plastics. XRD and SEM analyses confirm that the WhiteLite™ aluminosilicate powders are fully amorphous and contain no crystalline silica. Whitelite™ has an index of refraction that offers excellent clarity in clear polymer systems, and contributes to surface toughness in compounded polymers. The chemistry results in relative chemical inertness, making WhiteLite™ resistant to blooming, blistering, or chemical degradation in harsh environments. WhiteLite™ powders enhance a wide range of paints, coatings, plastics, and adhesives. High consistent brightness, tint retention and stain/scrub resistance can be achieved in most paint and coating systems. WhiteLite™ powders have low oil absorption and can be easily dispersed in water- or solvent-based systems. Vitro Minerals’ unique processing system and true particle size classification provides consistent product quality for 2 grades (WL-32, WL-42) with finenesses covering a range of potential applications. Under a microscope, WhiteLite™ particles are transparent, angular-shaped particles with similar dimensions in the x, y and z axis.

Information provided by Vitro Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.46 g/cc2.46 g/ccASMT D153
Bulk Density 0.641 g/cc0.0231 lb/in³ASTM C110
Brightness 90 - 91 %90 - 91 %Photovolt Y value
Oil Absorption 25 %25 %ASTM D281
Fineness 4.04.0Hegman; ASTM D-1210-79
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %Free; ASMT C566
Particle Size 6.0 - 7.0 µm6.0 - 7.0 µmd50 median; Laser interferometer
 40 µm40 µmd98 top; Laser interferometer
Particle Mesh Size 325 Mesh325 Mesh99.9%; ASTM C25
pH 6.0 - 8.06.0 - 8.0AFS 113-87-S
Specific Surface Area 2.5 m²/g2.5 m²/g
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.55.5
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 3500 ohm3500 ohmASTM D2448
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.501.50ASTM D801

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MasterSil 170 Gel Two component, addition curing silicone gel for sealing, potting and encapsulation
Master Bond MasterSil 157 Two component, addition curing silicone for potting, encapsulation and sealing
Master Bond MasterSil 151 Two Component Low Viscosity Silicone Compound
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Vitro Minerals WhiteLite™ 32 Lightweight Mineral Powder

CVITRO920 / 209594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.