MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schmolz + Bickenbach UGICHROM 4307 Austenitic Chrome Plated Bar
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced grades

Advantages: Zero defects guarantee; Low friction coefficient; High resistance to wear; Improved corrosion resistance; Micro-fissured chromium (1000 micro-fissures / cm²) guarantees a definitive level of resistance to extreme conditions in severe environments; Improved machinability (up to +20% of productivity); Superior mechanical properties; and High level of geometrical and dimensional precision

Information provided by Schmolz + Bickenbach

Key Words: EN 10088-3 1.4307; X2CrNi18-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 900
@Thickness 0.100 mm
900
@Thickness 0.00394 in
Tensile Strength at Break >= 450 MPa>= 65300 psi
Tensile Strength, Yield >= 175 MPa
@Strain 0.2 %
>= 25400 psi
@Strain 0.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
AISI 304L Cast Stainless Steel, EN 10088-3
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
301 Stainless Steel

NSCHMO057 / 125930

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.