MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling screws of blowers, electromotors, carrying parts in the automotive industry. Delivered in natural mode and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0034 cm/cm0.0034 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0068 cm/cm0.0068 in/inSTN 64 0808
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psiSTN EN ISO 527-2
Elongation at Break 2.0 %2.0 %STN EN ISO 527-2
Tensile Modulus 17.5 GPa2540 ksiSTN EN ISO 527-2
Flexural Strength 300 MPa43500 psiSTN EN ISO 178
Flexural Modulus 14.5 GPa2100 ksiSTN EN ISO 178
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -20.0 °C
42.8 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  1.50 J/cm²
@Temperature -20.0 °C
7.14 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FSTN EN ISO 75/A
Vicat Softening Point 210 °C410 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 90.0 - 100 °C194 - 212 °F
Drying Temperature 90.0 °C194 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 90.0 - 150 MPa13100 - 21800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry
EMS-Grivory Grivory® GVL-6H nat PA*-GF60
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60
Celanese SO.F.TER Nivionplast® BR60G PA66 compound, 60% GF

PPLACO015 / 106893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.