MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott LITHOTEC-CAF2 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 434952.318
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.18 g/cc0.115 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 4.54.5
Alkali Class, AR 2.32.3
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 158158.1/20
Modulus of Elasticity 76.0 GPa11000 ksi
Poissons Ratio 0.260.26
Shear Modulus 30.0 GPa4350 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  18.4 µm/m-°C
@Temperature -30.0 - 70.0 °C
10.2 µin/in-°F
@Temperature -22.0 - 158 °F
 21.3 µm/m-°C
@Temperature 20.0 - 300 °C
11.8 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.854 J/g-°C0.204 BTU/lb-°F
Thermal Conductivity 9.71 W/m-K67.4 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.43385
@Wavelength 587.6 nm
1.43385
@Wavelength 587.6 nm
nd
 1.43494
@Wavelength 546.1 nm
1.43494
@Wavelength 546.1 nm
ne
Abbe Number 94.6994.69ve
 95.2395.23vd
Optical Dispersion 0.0045560.004556nf - nc
 0.0045930.004593nf' - nc'
Transmission, Visible  99.9 %
@Thickness 10.0 mm,
Wavelength 380 nm
99.9 %
@Thickness 0.394 in,
Wavelength 380 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 405 nm
99.9 %
@Thickness 0.394 in,
Wavelength 405 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 460 nm
99.9 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.9 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.9 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  99.9 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.9 %
@Thickness 0.394 in,
Wavelength 1530 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 2500 nm
99.9 %
@Thickness 0.394 in,
Wavelength 2500 nm
UV Transmittance  99.9 %
@Thickness 10.0 mm,
Wavelength 270 nm
99.9 %
@Thickness 0.394 in,
Wavelength 270 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 300 nm
99.9 %
@Thickness 0.394 in,
Wavelength 300 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 334 nm
99.9 %
@Thickness 0.394 in,
Wavelength 334 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 370 nm
99.9 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B1
Climatic Resistance Test CR1
HG6
K (10-6mm2/N)1.77
Phosphate Resistance PR1.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO50 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO70 Temper flat products
Calcium Fluoride, CaF2 (Fluorite)
Aluminum 6061-T6; 6061-T651
MarkeTech Spinel (MgAl2O4) Single Crystal Substrate

CSGS103 / 93437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.