MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott LITHOTEC-CAF2 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 434952.318
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.18 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 4.5
Alkali Class, AR 2.3
Stain Resistance Class, FR 0.00
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 158.1/20
Modulus of Elasticity 76.0 GPa
Poissons Ratio 0.26
Shear Modulus 30.0 GPacalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.4 µm/m-°C
@Temperature -30.0 - 70.0 °C
 21.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.854 J/g-°C
Thermal Conductivity 9.71 W/m-K
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43385
@Wavelength 587.6 nm
nd
 1.43494
@Wavelength 546.1 nm
ne
Abbe Number 94.69ve
 95.23vd
Optical Dispersion 0.004556nf - nc
 0.004593nf' - nc'
Transmission, Visible 99.9 %
@Thickness 10.0 mm,
Wavelength 380 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 405 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 460 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 580 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 700 nm
IR Transmittance 99.9 %
@Thickness 10.0 mm,
Wavelength 1530 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 2500 nm
UV Transmittance 99.9 %
@Thickness 10.0 mm,
Wavelength 270 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 300 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 334 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 370 nm
 
Descriptive Properties
B1
Climatic Resistance Test CR1
HG6
K (10-6mm2/N)1.77
Phosphate Resistance PR1.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO50 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO70 Temper flat products
Calcium Fluoride, CaF2 (Fluorite)
Aluminum 6061-T6; 6061-T651
MarkeTech Spinel (MgAl2O4) Single Crystal Substrate

CSGS103 / 93437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.