MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hyosung Topilene C600 PP
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: C600 Film Grade Butane Random Copolymer

Applications: Metallizing CPP

Characteristics:

  • Al bonding strength
  • High gloss

Information provided by Hyosung Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 30.4 MPa4410 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 1.08 GPa156 ksiASTM D790
Izod Impact, Unnotched 0.490 J/cm0.918 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FHS Method
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D648
Vicat Softening Point 140 °C284 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hyosung Topilene C600MU PP
Hyosung Topilene C600ME PP
Hyosung Topilene C600M3 PP
Hyosung Topilene C600M2 PP
Hyosung Topilene C600M PP

PHYOS40 / 47926

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.