System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Hyosung Topilene C600 PP
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Film Grade
Material Notes:
C600 Film Grade Butane Random Copolymer
Applications:
Metallizing CPP
Characteristics:
Al bonding strength
High gloss
Information provided by Hyosung Corporation
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Melt Flow
7.0
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
85
ASTM D785
Tensile Strength, Yield
310
kg(f)/cm²
ASTM D638
Elongation at Break
500 %
ASTM D638
Flexural Modulus
11000
kg(f)/cm²
ASTM D790
Izod Impact, Unnotched
5.00
kg-cm/cm
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
150
°C
HS Method
Deflection Temperature at 0.46 MPa (66 psi)
100
°C
ASTM D648
Vicat Softening Point
140
°C
ASTM D1525
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Hyosung Topilene C600MU PP
Hyosung Topilene C600ME PP
Hyosung Topilene C600M3 PP
Hyosung Topilene C600M2 PP
Hyosung Topilene C600M PP
PHYOS40 / 47926
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.