MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Accella ECOBAY® CC Polyurethane Spray Foam Insulation
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: EcoBay CC closed-cell is a spray-applied polyurethane foam (SPF) insulation.

Properties / Applications: EcoBay CC closed cell spray applied polyurethane foam insulation is produced from a two component, HFC-245fa blown, medium density, structural system designed for commercial applications. EcoBay CC closed cell spray-applied polyurethane forms an integral part of any air barrier system. The EcoBay CC foam is made with an "A" component or aromatic diisocyanate and a blended "B" component which includes polyols, fire retarding materials, and additives. Both components are manufactured by Covestro LLC. EcoBay CC foam is available in two grades for warm and cold weather applications

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0300 - 0.0350 g/cc0.0300 - 0.0350 g/ccASTM D1622
Water Absorption <= 2.0 %<= 2.0 %ASTM D2842
Viscosity 150 - 250 cP150 - 250 cPComponent A
 400 - 500 cP400 - 500 cPComponent B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.414 MPa60.0 psiASTM D1623
Compressive Strength 0.172 MPa24.9 psiASTM D1621
Adhesive Bond Strength >= 0.110 MPa>= 16.0 psiExterior Gypsum Board; ASTM D4541
 >= 0.200 MPa>= 29.0 psiMetal Deck, primed/washed; ASTM D4541
 >= 0.200 MPa>= 29.0 psiOSB, Wood Studs, Plywood; ASTM D4541
 >= 0.241 MPa>= 35.0 psiCMU; ASTM D4541
 >= 0.303 MPa>= 44.0 psiPrecast Concrete; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
Insulation R Value  6.9
@Thickness 25.4 mm
6.9
@Thickness 1.00 in
Aged 6 months; ASTM C-518
 24.1
@Thickness 88.9 mm
24.1
@Thickness 3.50 in
Aged 6 months; ASTM C-518

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Accella ECOBAY® CC CAN Polyurethane Spray Foam Insulation
Covestro Baynat® 3002 Polyurethane Foam
Overview of materials for Polypropylene Glass Bead Filled
Overview of materials for Polypropylene Copolymer
Graphite, Carbon, C

PCOVEST0776 / 202559

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.