MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene Glass Bead Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Glass Bead Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.770 - 1.40 g/cc0.0278 - 0.0506 lb/in³Average value: 1.09 g/cc Grade Count:39
Filler Content 20.0 - 50.0 %20.0 - 50.0 %Average value: 33.3 % Grade Count:3
Water Absorption 0.0200 - 0.0500 %0.0200 - 0.0500 %Average value: 0.0271 % Grade Count:14
Additive Loading 10.0 - 40.0 %10.0 - 40.0 %Average value: 25.0 % Grade Count:4
Maximum Moisture Content  0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:2
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:2
Linear Mold Shrinkage 0.00600 - 0.0226 cm/cm0.00600 - 0.0226 in/inAverage value: 0.0138 cm/cm Grade Count:32
Linear Mold Shrinkage, Transverse 0.00600 - 0.0210 cm/cm0.00600 - 0.0210 in/inAverage value: 0.0138 cm/cm Grade Count:14
Melt Flow 3.00 - 25.0 g/10 min3.00 - 25.0 g/10 minAverage value: 9.77 g/10 min Grade Count:20
Ash 28.0 - 42.0 %
@Temperature 625 - 625 °C
28.0 - 42.0 %
@Temperature 1160 - 1160 °F
Average value: 35.0 % Grade Count:2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 89.0 - 10089.0 - 100Average value: 96.2 Grade Count:10
Tensile Strength, Ultimate 6.21 - 37.0 MPa900 - 5370 psiAverage value: 23.4 MPa Grade Count:28
Tensile Strength, Yield 16.0 - 26.2 MPa2320 - 3800 psiAverage value: 21.5 MPa Grade Count:12
Elongation at Break 2.00 - 100 %2.00 - 100 %Average value: 25.5 % Grade Count:32
Elongation at Yield 3.40 - 100 %3.40 - 100 %Average value: 15.5 % Grade Count:11
Modulus of Elasticity 1.10 - 3.25 GPa160 - 471 ksiAverage value: 1.95 GPa Grade Count:31
Flexural Yield Strength 10.3 - 55.0 MPa1500 - 7980 psiAverage value: 36.4 MPa Grade Count:32
Flexural Modulus 1.03 - 3.10 GPa149 - 450 ksiAverage value: 1.89 GPa Grade Count:34
Compressive Yield Strength 29.0 - 34.5 MPa4200 - 5000 psiAverage value: 32.1 MPa Grade Count:4
Izod Impact, Notched 0.160 - 1.60 J/cm0.300 - 3.00 ft-lb/inAverage value: 0.402 J/cm Grade Count:22
 0.200 - 0.200 J/cm
@Temperature -20.0 - -20.0 °C
0.375 - 0.375 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.200 J/cm Grade Count:1
Izod Impact, Unnotched 0.300 - 10.7 J/cm0.562 - 20.0 ft-lb/inAverage value: 4.06 J/cm Grade Count:14
 0.200 - 0.200 J/cm
@Temperature 0.000 - 0.000 °C
0.375 - 0.375 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.200 J/cm Grade Count:1
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²1.28 - 2.86 ft-lb/in²Average value: 3.90 kJ/m² Grade Count:3
 4.00 - 4.00 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 1.90 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.50 - 6.00 J/cm²7.14 - 28.6 ft-lb/in²Average value: 3.42 J/cm² Grade Count:12
 1.80 - 3.40 J/cm²
@Temperature -20.0 - -20.0 °C
8.57 - 16.2 ft-lb/in²
@Temperature -4.00 - -4.00 °F
Average value: 2.44 J/cm² Grade Count:5
Charpy Impact, Notched 0.250 - 0.600 J/cm²1.19 - 2.86 ft-lb/in²Average value: 0.423 J/cm² Grade Count:14
 0.200 - 0.500 J/cm²
@Temperature -30.0 - -20.0 °C
0.952 - 2.38 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.353 J/cm² Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+17 ohm-cm1.00e+12 - 1.00e+17 ohm-cmAverage value: 1.37e+16 ohm-cm Grade Count:14
Surface Resistance 1.00e+12 - 1.00e+15 ohm1.00e+12 - 1.00e+15 ohmAverage value: 3.67e+14 ohm Grade Count:3
Dielectric Strength 19.7 kV/mm500 kV/inAverage value: 19.7 kV/mm Grade Count:6
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 - 68.0 µm/m-°C21.0 - 37.8 µin/in-°FAverage value: 58.4 µm/m-°C Grade Count:9
Melting Point 150 - 170 °C302 - 338 °FAverage value: 164 °C Grade Count:15
Deflection Temperature at 0.46 MPa (66 psi) 76.0 - 145 °C169 - 293 °FAverage value: 116 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 56.0 - 160 °C133 - 320 °FAverage value: 76.5 °C Grade Count:31
Vicat Softening Point 64.0 - 156 °C147 - 313 °FAverage value: 105 °C Grade Count:15
Flammability, UL94 HBHBGrade Count:17
Oxygen Index 20.0 - 21.0 %20.0 - 21.0 %Average value: 20.7 % Grade Count:3
Glow Wire Test 550 - 650 °C1020 - 1200 °FAverage value: 625 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 240 °C380 - 464 °FAverage value: 211 °C Grade Count:7
Melt Temperature 160 - 270 °C320 - 518 °FAverage value: 219 °C Grade Count:22
Mold Temperature 20.0 - 90.0 °C68.0 - 194 °FAverage value: 51.7 °C Grade Count:29
Drying Temperature 79.4 - 120 °C175 - 248 °FAverage value: 89.5 °C Grade Count:17
Injection Pressure 60.0 - 120 MPa8700 - 17400 psiAverage value: 87.9 MPa Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
Overview of materials for Polypropylene with 10% Glass Fiber Filler

O4717 / 78382

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.