LE0315 is an Easy Strippable Semi conductive Insulation Shield for EPR Insulated, Medium Voltage (5-46 kV) Cables. Strip forces range from 5 to 10 lbs/0.5". Specifications: LE0315 meets the applicable requirements below using sound commercial extrusion practice and testing procedures: AEIC CS8-00 (1st edition); ICEA S-94-649; and ICEA S-97-682Information provided by Borealis AG |