MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borlink™ LE0315 Polyethylene Compound, Crosslinkable, Semiconductive
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0315 is an Easy Strippable Semi conductive Insulation Shield for EPR Insulated, Medium Voltage (5-46 kV) Cables. Strip forces range from 5 to 10 lbs/0.5". Specifications: LE0315 meets the applicable requirements below using sound commercial extrusion practice and testing procedures: AEIC CS8-00 (1st edition); ICEA S-94-649; and ICEA S-97-682

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11.0 MPaASTM D638
Elongation at Break <= 75 %after aging 168h @ 136°C; ASTM D638
 250 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 ohm-cm
@Temperature 23.0 °C
ASTM D991
 100 ohm-cm
@Temperature 90.0 °C
ASTM D991
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables
Borealis Borlink™ LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Borealis Borlink™ LE0315-99 Polyethylene Thermoplastic Semiconductive Compound

PBOREA504 / 108763

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.