MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYAXIS® CP813-31 General-Purpose Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: Description

Polyaxis CP 813-31 is a general-purpose black linear low density polyethylene compound offering quick cycles and part to part consistency.

NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.935 g/cc0.935 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D1693
Melt Index of Compound 5.5 - 7.0 g/10 min5.5 - 7.0 g/10 min2.16/190; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 15.9 MPa2300 psi2"/min; ASTM D638
Elongation at Break 400 %400 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 538 MPa78000 psiASTM D790
Impact Test 54.2 J
@Thickness 3.17 mm,
Temperature -40.0 °C
40.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °C120 °FASTM D648
 
Descriptive Properties
UV StabilizationUV-8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global PP-100 General Purpose Polypropylene Homopolymer, Controlled Rheology
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding
Polymer Resources ABS-GP1 General Purpose ABS
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Braskem ML3601U LLDPE Rotomolding Polyethylene

PASHU062 / 25026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.