MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources ABS-GP1 General Purpose ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: General Purpose Acrylonitrile Butadiene Styrene

Features: • Medium Impact Resistance
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 3.0 - 14 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.0 - 14 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength at Break 39.3 MPa5700 psiASTM D638
Tensile Strength, Yield 42.1 MPa6100 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
Tensile Modulus 2.62 GPa380 ksiASTM D638
Flexural Strength 64.1 MPa9300 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched  0.534 J/cm
@Temperature -40.0 °C
1.00 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 2.14 J/cm
@Temperature 22.8 °C
4.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  7.35 kJ/m²
@Temperature -30.0 °C
3.50 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 16.4 kJ/m²
@Temperature 22.8 °C
7.80 ft-lb/in²
@Temperature 73.0 °F
ISO 180/1A
Charpy Impact, Notched 1.89 J/cm²
@Temperature 22.8 °C
9.00 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
Gardner Impact 22.6 J16.7 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C190 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D648
Vicat Softening Point 98.9 °C210 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical  60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
UL 746
 60.0 °C
@Thickness 3.00 mm
140 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
UL 746
 60.0 °C
@Thickness 3.00 mm
140 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  60.0 °C
@Thickness 1.50 mm
140 °F
@Thickness 0.0591 in
UL 746
 60.0 °C
@Thickness 3.00 mm
140 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 188 - 210 °C370 - 410 °F
Middle Barrel Temperature 204 - 227 °C400 - 440 °F
Front Barrel Temperature 216 - 238 °C420 - 460 °F
Melt Temperature 232 - 260 °C450 - 500 °F
Mold Temperature 48.9 - 71.1 °C120 - 160 °F
Drying Temperature 82.2 - 93.3 °C180 - 200 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00254 cm0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 484 High Impact Polystyrene
AlphaGary Evoprene™ Super G 932 SEBS Thermoplastic Elastomer
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene
A. Schulman PP 3479-01 Polypropylene Random Copolymer
A. Schulman Matrixx 15A4201 Flame Retardant 20% Talc Filled Polypropylene (5VA)

PPOLYQ008 / 160522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.