MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess CERES® Blue XR-RF Gran Dye Mixture
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Main fields of application: Special dyestuff for the coloring of PET X-Ray film layer.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.460 g/cc0.0166 lb/in³DIN ISO 787-11
Density 1.26 g/cc0.0455 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 167 °C333 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  20 %
@Thickness 2.00 mm,
Wavelength 630 nm
20 %
@Thickness 0.0787 in,
Wavelength 630 nm
0.01% dyestuff
 22 %
@Thickness 2.00 mm,
Wavelength 590 nm
22 %
@Thickness 0.0787 in,
Wavelength 590 nm
0.01% dyestuff
 28 %
@Thickness 2.00 mm,
Wavelength 610 nm
28 %
@Thickness 0.0787 in,
Wavelength 610 nm
0.01% dyestuff
 59 %
@Thickness 2.00 mm,
Wavelength 640 nm
59 %
@Thickness 0.0787 in,
Wavelength 640 nm
0.003% dyestuff
 61 %
@Thickness 2.00 mm,
Wavelength 570 nm
61 %
@Thickness 0.0787 in,
Wavelength 570 nm
0.003% dyestuff
 65 %
@Thickness 2.00 mm,
Wavelength 610 nm
65 %
@Thickness 0.0787 in,
Wavelength 610 nm
0.003% dyestuff
 75 %
@Thickness 2.00 mm,
Wavelength 360 nm
75 %
@Thickness 0.0787 in,
Wavelength 360 nm
0.01% dyestuff
 82 %
@Thickness 2.00 mm,
Wavelength 400 nm
82 %
@Thickness 0.0787 in,
Wavelength 400 nm
0.003% dyestuff
 85 %
@Thickness 2.00 mm,
Wavelength 460 nm
85 %
@Thickness 0.0787 in,
Wavelength 460 nm
0.01% dyestuff
 86 %
@Thickness 2.00 mm,
Wavelength 460 nm
86 %
@Thickness 0.0787 in,
Wavelength 460 nm
0.003% dyestuff
 88 %
@Thickness 2.00 mm,
Wavelength 680 nm
88 %
@Thickness 0.0787 in,
Wavelength 680 nm
0.003% dyestuff
 90 %
@Thickness 2.00 mm,
Wavelength 720 nm
90 %
@Thickness 0.0787 in,
Wavelength 720 nm
0.003% dyestuff
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month60.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidiemme® G/430 Polyolefin
Syensqo (Solvay Specialty Polymers) Polidiemme® G/450 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/400 Thermoset Elastomer (TSE)
Solvay Chemicals NOCOLOK® Sil Flux (extra fine grade) plus Binder Mixture
BASF Pentanol Mixture

PLANY8528 / 208921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.