MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Polidiemme® G/400 Thermoset Elastomer (TSE)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polidiemme® XLPO -Cross-linkable Polyolefin

Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method).

Standard complying

- EN 50363-1 EI4, EI6 and EI7; EN 50363-2 EM3 and EM6; Cenelec HD 603 DIH1; BS 7655 GP4, GP5 and GP7; IEC 60092/360 EPR; IEC 60502 EPR; VDE 0207/20 3GI3

Crosslinkable; Good Flexibility; Low Toxicity

Uses: Cable Jacketing; Low Voltage Insulation; Wire & Cable Applications

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 2323ISO 868
Tensile Strength at Break 12.0 MPa1740 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Tear Strength 8.00 kN/m45.6 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  2.70e+14 ohm-cm
@Temperature 90.0 °C
2.70e+14 ohm-cm
@Temperature 194 °F
ASTM D257
 4.10e+15 ohm-cm
@Temperature 20.0 °C
4.10e+15 ohm-cm
@Temperature 68.0 °F
ASTM D257
Dielectric Constant 2.3
@Frequency 1000 Hz
2.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 33.0 kV/mm838 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 
Processing PropertiesMetricEnglishComments
Zone 1 120 - 140 °C248 - 284 °F
Zone 2 120 - 150 °C248 - 302 °F
Zone 3 130 - 160 °C266 - 320 °F
Zone 4 140 - 170 °C284 - 338 °F
Die Temperature 140 - 170 °C284 - 338 °F
 
Descriptive Properties
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidiemme® G/430 Polyolefin
Syensqo (Solvay Specialty Polymers) Polidiemme® G/450 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/440 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/320 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/360 Polyolefin

PSOL8Y6317 / 193238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.