MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Thermoplastic Polyimide, Carbon Fiber
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Carbon Fiber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.38 - 1.68 g/cc0.0499 - 0.0607 lb/in³Average value: 1.48 g/cc Grade Count:14
Filler Content 20.0 - 30.0 %20.0 - 30.0 %Average value: 26.7 % Grade Count:3
Water Absorption 0.660 - 0.660 %
@Temperature 80.0 - 80.0 °C
0.660 - 0.660 %
@Temperature 176 - 176 °F
Average value: 1.71 % Grade Count:1
 2.24 - 2.24 %
@Temperature 80.0 - 80.0 °C
2.24 - 2.24 %
@Temperature 176 - 176 °F
Average value: 1.71 % Grade Count:1
 2.24 - 2.24 %
@Time 86400 - 86400 sec
2.24 - 2.24 %
@Time 24.0 - 24.0 hour
Average value: 1.71 % Grade Count:1
Water Absorption at Saturation 4.17 - 4.17 %
@Temperature 80.0 - 80.0 °C
4.17 - 4.17 %
@Temperature 176 - 176 °F
Average value: 4.17 % Grade Count:1
Linear Mold Shrinkage 0.000100 - 0.00300 cm/cm0.000100 - 0.00300 in/inAverage value: 0.00171 cm/cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 89.0 - 91.089.0 - 91.0Average value: 90.0 Grade Count:3
Tensile Strength, Ultimate 36.5 - 241 MPa5300 - 35000 psiAverage value: 158 MPa Grade Count:8
 97.0 - 130 MPa
@Temperature 260 - 260 °C
14100 - 18900 psi
@Temperature 500 - 500 °F
Average value: 112 MPa Grade Count:3
Elongation at Break 0.800 - 5.50 %0.800 - 5.50 %Average value: 2.17 % Grade Count:6
Modulus of Elasticity 4.50 - 29.0 GPa653 - 4200 ksiAverage value: 18.1 GPa Grade Count:9
Flexural Yield Strength 97.9 - 345 MPa14200 - 50000 psiAverage value: 212 MPa Grade Count:11
 165 - 195 MPa
@Temperature 260 - 260 °C
23900 - 28300 psi
@Temperature 500 - 500 °F
Average value: 175 MPa Grade Count:3
Flexural Modulus 4.24 - 25.5 GPa615 - 3700 ksiAverage value: 14.3 GPa Grade Count:11
 15.0 - 17.0 GPa
@Temperature 260 - 260 °C
2180 - 2470 ksi
@Temperature 500 - 500 °F
Average value: 16.0 GPa Grade Count:3
Flexural Strain at Yield 2.60 - 4.30 %2.60 - 4.30 %Average value: 3.27 % Grade Count:3
Compressive Yield Strength 184 - 474 MPa26700 - 68700 psiAverage value: 279 MPa Grade Count:4
Izod Impact, Notched 0.801 - 1.07 J/cm1.50 - 2.00 ft-lb/inAverage value: 0.921 J/cm Grade Count:4
Izod Impact, Unnotched 4.81 - 6.41 J/cm9.00 - 12.0 ft-lb/inAverage value: 5.94 J/cm Grade Count:4
Compression Set 49.0 - 98.0 %49.0 - 98.0 %Average value: 69.0 % Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 41.0 - 88.0 µm/m-°C
@Temperature 50.0 - 300 °C
22.8 - 48.9 µin/in-°F
@Temperature 122 - 572 °F
Average value: 61.0 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 43.0 - 67.0 µm/m-°C
@Temperature 50.0 - 300 °C
23.9 - 37.2 µin/in-°F
@Temperature 122 - 572 °F
Average value: 54.5 µm/m-°C Grade Count:2
Deflection Temperature at 1.8 MPa (264 psi) 316 °C600 °FAverage value: 316 °C Grade Count:3
Glass Transition Temp, Tg 330 - 360 °C626 - 680 °FAverage value: 350 °C Grade Count:7
Flammability, UL94 V-0V-0Grade Count:5
 
Processing PropertiesMetricEnglishComments
Melt Temperature 399 - 416 °C750 - 780 °FAverage value: 407 °C Grade Count:3
Mold Temperature 177 - 232 °C350 - 450 °FAverage value: 204 °C Grade Count:4
Drying Temperature 204 °C400 °FAverage value: 204 °C Grade Count:3
Moisture Content 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:3
Dew Point -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:3
Injection Pressure 138 - 193 MPa20000 - 28000 psiAverage value: 165 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyimide, Unfilled
Overview of materials for Polyimide
Overview of materials for Polyimide, Graphite Filled
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Polyimide, Thermoset Film

O4220 / 78307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.