MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Carbon Fiber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.38 - 1.68 g/ccAverage value: 1.48 g/cc Grade Count:14
Filler Content 20.0 - 30.0 %Average value: 26.7 % Grade Count:3
Water Absorption 0.660 - 0.660 %
@Temperature 80.0 - 80.0 °C
Average value: 1.71 % Grade Count:1
 2.24 - 2.24 %
@Temperature 80.0 - 80.0 °C
Average value: 1.71 % Grade Count:1
 2.24 - 2.24 %
@Time 86400 - 86400 sec
Average value: 1.71 % Grade Count:1
Water Absorption at Saturation 4.17 - 4.17 %
@Temperature 80.0 - 80.0 °C
Average value: 4.17 % Grade Count:1
Linear Mold Shrinkage 0.000100 - 0.00300 cm/cmAverage value: 0.00171 cm/cm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89.0 - 91.0Average value: 90.0 Grade Count:3
Tensile Strength, Ultimate 36.5 - 241 MPaAverage value: 158 MPa Grade Count:8
 97.0 - 130 MPa
@Temperature 260 - 260 °C
Average value: 112 MPa Grade Count:3
Elongation at Break 0.800 - 5.50 %Average value: 2.17 % Grade Count:6
Modulus of Elasticity 4.50 - 29.0 GPaAverage value: 18.1 GPa Grade Count:9
Flexural Yield Strength 97.9 - 345 MPaAverage value: 212 MPa Grade Count:11
 165 - 195 MPa
@Temperature 260 - 260 °C
Average value: 175 MPa Grade Count:3
Flexural Modulus 4.24 - 25.5 GPaAverage value: 14.3 GPa Grade Count:11
 15.0 - 17.0 GPa
@Temperature 260 - 260 °C
Average value: 16.0 GPa Grade Count:3
Flexural Strain at Yield 2.60 - 4.30 %Average value: 3.27 % Grade Count:3
Compressive Yield Strength 184 - 474 MPaAverage value: 279 MPa Grade Count:4
Izod Impact, Notched 0.801 - 1.07 J/cmAverage value: 0.921 J/cm Grade Count:4
Izod Impact, Unnotched 4.81 - 6.41 J/cmAverage value: 5.94 J/cm Grade Count:4
Compression Set 49.0 - 98.0 %Average value: 69.0 % Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 41.0 - 88.0 µm/m-°C
@Temperature 50.0 - 300 °C
Average value: 61.0 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 43.0 - 67.0 µm/m-°C
@Temperature 50.0 - 300 °C
Average value: 54.5 µm/m-°C Grade Count:2
Deflection Temperature at 1.8 MPa (264 psi) 316 °CAverage value: 316 °C Grade Count:3
Glass Transition Temp, Tg 330 - 360 °CAverage value: 350 °C Grade Count:7
Flammability, UL94 V-0Grade Count:5
 
Processing PropertiesOriginal ValueComments
Melt Temperature 399 - 416 °CAverage value: 407 °C Grade Count:3
Mold Temperature 177 - 232 °CAverage value: 204 °C Grade Count:4
Drying Temperature 204 °CAverage value: 204 °C Grade Count:3
Moisture Content 0.0100 %Average value: 0.0100 % Grade Count:3
Dew Point -40.0 °CAverage value: -40.0 °C Grade Count:3
Injection Pressure 138 - 193 MPaAverage value: 165 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyimide, Unfilled
Overview of materials for Polyimide
Overview of materials for Polyimide, Graphite Filled
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Polyimide, Thermoset Film

O4220 / 78307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.