System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 610 (PA610)
;
Nylon 610, Glass Reinforced
Material Notes:
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.31
g/cc
0.0473
lb/in³
Linear Mold Shrinkage, Flow
0.0035
-
0.0065
cm/cm
0.0035
-
0.0065
in/in
Linear Mold Shrinkage, Transverse
0.0075
-
0.0105
cm/cm
0.0075
-
0.0105
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
70.0
MPa
@Temperature 150 °C
10200
psi
@Temperature 302 °F
85.0
MPa
@Temperature 120 °C
12300
psi
@Temperature 248 °F
100
MPa
@Temperature 90.0 °C
14500
psi
@Temperature 194 °F
120
MPa
@Temperature 60.0 °C
17400
psi
@Temperature 140 °F
165
MPa
@Temperature 23.0 °C
23900
psi
@Temperature 73.4 °F
Elongation at Break
3.2 %
@Temperature 23.0 °C
3.2 %
@Temperature 73.4 °F
4.2 %
@Temperature 60.0 °C
4.2 %
@Temperature 140 °F
4.9 %
@Temperature 90.0 °C
4.9 %
@Temperature 194 °F
5.4 %
@Temperature 120 °C
5.4 %
@Temperature 248 °F
6.1 %
@Temperature 150 °C
6.1 %
@Temperature 302 °F
Tensile Modulus
3.00
GPa
@Temperature 150 °C
435
ksi
@Temperature 302 °F
3.60
GPa
@Temperature 120 °C
522
ksi
@Temperature 248 °F
5.30
GPa
@Temperature 90.0 °C
769
ksi
@Temperature 194 °F
6.20
GPa
@Temperature 60.0 °C
899
ksi
@Temperature 140 °F
8.80
GPa
@Temperature 23.0 °C
1280
ksi
@Temperature 73.4 °F
Charpy Impact Unnotched
10.0
J/cm²
47.6
ft-lb/in²
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
120
°C
248
°F
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
428
°F
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
Vicat Softening Point
220
°C
@Load 5.00 kg
428
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
260
-
280
°C
500
-
536
°F
Mold Temperature
80.0
-
100
°C
176
-
212
°F
Drying Temperature
70.0
-
90.0
°C
@Time 10800 sec
158
-
194
°F
@Time 3.00 hour
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
EMS-Grivory Grilamid® XE 4104 nat PA610-GF40
EMS-Grivory Grilamid® 2SV-30H nat PA610-GF30
Domo TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, Conditioned
BASF Ultramid® TG3S 15% Glass Filled PA6 (Conditioned)
PLATH9741 / 177437
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.