MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Domo TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: TECHNYL® eXten D 218 V30 is suitable to the manufacturing of injection molded parts in all sectors of applications. It offers excellent chemical resistance, low water absorption, very good mechanical properties and mold ability.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183/A
Linear Mold Shrinkage, Flow 0.035 cm/cm0.035 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.070 cm/cm0.070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 72.0 MPa10400 psiISO 527 Type 1A
Elongation at Break 8.0 %8.0 %ISO 527 Type 1A
Tensile Modulus 5.50 GPa798 ksiISO 527 Type 1A
Charpy Impact Unnotched 8.50 J/cm²40.5 ft-lb/in²ISO 179/1eU
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0

PRHOD552 / 137783

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.