MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell ArmaFORM® PET Foil 70
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Armacell PET foil is designed to provide a highly sustainable and improved alternative to cross-linked XPE and XPP products currently available in the market.
  • improved stiffness and compression
  • very smooth surface (closed and fine cells)
  • high resistance to solvents
  • service temperature -38F to +365F
  • broader thermoforming window
  • easy processing and shaping
  • made from 100% recycled PET
  • 100% recyclable after use
  • significantly reduced CO2 emission and energy consumption

Information provided by Armacell®

Key Words: Green; recyclable
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0705 g/cc0.00255 lb/in³ISO 845
Thickness 4060 - 5080 microns160 - 200 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 80 %80 %
Film Elongation at Break, TD 30 %30 %
Film Tensile Strength at Break, MD 1.69 MPa245 psi
Film Tensile Strength at Break, TD 1.59 MPa230 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -38.9 °C-38.0 °F
 
Descriptive Properties
FMVVSS 302PASS; <100mm/minAutomotive standard
Tear StrengthMD: 2175 psiAutomotive standard
 TD: 2610 psiAutomotive standard

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell ArmaForm® PET Foil 70
Solvay P720X PET-Based Release Film
Armacell ArmaFORM® PET Foil 300
Armacell ArmaFORM® PET Foil 120
Eastman 9921P PET Film

PARMC12 / 183704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.